Paramèt teknik
Tablo 1: Paramèt teknik pou ti Dyamèt Graphite Electrode
Dyamèt | Pati | Rezistans | Fòs flexural | Modil jèn | Dansite | CTE | Ash | |
Pous | mm | μΩ·m | MPa | GPa | g/cm3 | ×10-6/℃ | % | |
3 | 75 | Elektwòd | 7.5-8.5 | ≥9.0 | ≤9.3 | 1.55-1.64 | ≤2.4 | ≤0.3 |
Pwent tete | 5.8-6.5 | ≥16.0 | ≤13.0 | ≥1.74 | ≤2.0 | ≤0.3 | ||
4 | 100 | Elektwòd | 7.5-8.5 | ≥9.0 | ≤9.3 | 1.55-1.64 | ≤2.4 | ≤0.3 |
Pwent tete | 5.8-6.5 | ≥16.0 | ≤13.0 | ≥1.74 | ≤2.0 | ≤0.3 | ||
6 | 150 | Elektwòd | 7.5-8.5 | ≥8.5 | ≤9.3 | 1.55-1.63 | ≤2.4 | ≤0.3 |
Pwent tete | 5.8-6.5 | ≥16.0 | ≤13.0 | ≥1.74 | ≤2.0 | ≤0.3 | ||
8 | 200 | Elektwòd | 7.5-8.5 | ≥8.5 | ≤9.3 | 1.55-1.63 | ≤2.4 | ≤0.3 |
Pwent tete | 5.8-6.5 | ≥16.0 | ≤13.0 | ≥1.74 | ≤2.0 | ≤0.3 | ||
9 | 225 | Elektwòd | 7.5-8.5 | ≥8.5 | ≤9.3 | 1.55-1.63 | ≤2.4 | ≤0.3 |
Pwent tete | 5.8-6.5 | ≥16.0 | ≤13.0 | ≥1.74 | ≤2.0 | ≤0.3 | ||
10 | 250 | Elektwòd | 7.5-8.5 | ≥8.5 | ≤9.3 | 1.55-1.63 | ≤2.4 | ≤0.3 |
Pwent tete | 5.8-6.5 | ≥16.0 | ≤13.0 | ≥1.74 | ≤2.0 | ≤0.3 |
Tablo 2: Kapasite aktyèl pou pote ti Dyamèt Graphite Electrode
Dyamèt | Chaj aktyèl | Dansite aktyèl la | Dyamèt | Chaj aktyèl | Dansite aktyèl la | ||
Pous | mm | A | A/m2 | Pous | mm | A | A/m2 |
3 | 75 | 1000-1400 | 22-31 | 6 | 150 | 3000-4500 | 16-25 |
4 | 100 | 1500-2400 | 19-30 | 8 | 200 | 5000-6900 | 15-21 |
5 | 130 | 2200-3400 | 17-26 | 10 | 250 | 7000-10000 | 14-20 |
Tablo 3: Graphite Electrode Size & Tolerans Pou Ti Dyamèt Graphite Electrode
Dyamèt nominal | Dyamèt aktyèl (mm) | Longè nominal | Tolerans | |||
Pous | mm | Max. | Min. | mm | Pous | mm |
3 | 75 | 77 | 74 | 1000 | 40 | -75 ~ + 50 |
4 | 100 | 102 | 99 | 1200 | 48 | -75 ~ + 50 |
6 | 150 | 154 | 151 | 1600 | 60 | ± 100 |
8 | 200 | 204 | 201 | 1600 | 60 | ± 100 |
9 | 225 | 230 | 226 | 1600/1800 | 60/72 | ± 100 |
10 | 250 | 256 | 252 | 1600/1800 | 60/72 | ± 100 |
Aplikasyon prensipal la
- carbure kalsyòm fusion
- Pwodiksyon Carborundum
- Corundum raffinage
- Metal ra fusion
- Ferrosilicon plant refractory
Distribisyon enstriksyon ak itilizasyon pou elektwòd grafit
1.Sèvi ak zouti espesyal pou leve elektwòd grafit la, evite domaje pandan transpò. (gade pic1)
2.Lektwòd grafit dwe kenbe lwen ke yo te mouye oswa mouye pa lapli, nèj, dwe kenbe sèk. (gade pic2)
3.Atansyon tcheke anvan ou itilize asire priz la ak fil pwent tete a apwopriye pou itilize, ki gen ladan enspeksyon pou anplasman, ploge. (gade pic3)
4.Netwaye pwent tete a ak fil sipò yo pa lè konprese. (gade pic4)
5.Anvan itilize, elektwòd grafit la dwe cheche nan gwo fou a, tanperati siye a ta dwe mwens pase 150 ℃, tan an seche yo ta dwe plis pase 30 èdtan. (gade pic5)
6.Lektwòd grafit dwe konekte byen sere ak dwat ak koupl apwopriye pou sere. (gade pic6)
7.Pou evite kraze elektwòd grafit la, mete gwo pati a nan pozisyon ki pi ba ak ti pati nan pozisyon anwo a.